Abstract
The present publication describes a process and structure to selectively create higher-melting-temperature solder bumps in specific locations on integrated circuit packages subject to head-in-pillow (HiP) solder defects. By utilizing an intermediate solder paste formed from an alloy having a melting temperature lower than that of the opposed solder bumps, the assembly reflow temperature is controlled to melt the intermediate solder paste without liquefying the higher-melting-temperature solder bumps. Consequently, the higher-melting-temperature solder bumps retain their solid geometric shape to preserve standoff height across high-separation regions, and the molten lower-melting-temperature solder paste wets and solidifies between the bumps to establish a continuous metallurgical joint. Keywords: dynamic warpage, head-in-pillow, HiP, non-contact open, pre-bumped printed circuit board, PCB, multi-alloy solder joint, selective solder deposition, area ratio, ball grid array, solder, ASIC, integrated circuit, integrated circuit package.
Creative Commons License

This work is licensed under a Creative Commons Attribution 4.0 License.
Recommended Citation
N/A and , "Trio-Solder Joint", Technical Disclosure Commons, ()
https://www.tdcommons.org/dpubs_series/13357