When we make a shining chamfer/surface in magnesium part, the cutting chamfer/surface is easily fogging and

corroded. We take some actions to avoid the fogging and corrosion. This patent is an overall effective solution. Prior

shining chamfer/surface is used in Al metal parts, not in magnesium material. Because Mg material is easily corroded

and cutting chamfer/surface is not shining than Al material. Prior solution is using chemical conversion and ED (Electro

Deposition) to protect cutting surface and avoid corrosion, keep the shining surface as same as Al material part.